Research Update: Atmospheric pressure spatial atomic layer deposition of ZnO thin films: Reactors, doping, and devices
Atmospheric pressure spatial atomic layer deposition (AP-SALD) has recently emerged as an appealing technique for rapidly producing high quality oxides. Here, we focus on the use of AP-SALD to deposit functional ZnO thin films, particularly on the reactors used, the film properties, and the dopants
Conceptio Open Archive
Analyze & explore related research in Conceptio
Connect this record directly into your research workflow or AI agent. Explore citations across open repositories, query full text, and export structured proof bundles.
This document is indexed with metadata only: full text is not available in the archive for this record. Open the official source ↗
Related documents
- Enhancing Thermoelectric Performance: The Impact of Carbon Incorporation in Spin-Coated Al-Doped ZnO Thin Films#205725
- Tailoring ZnO thin films via ALD: Impact of cycle number on structural, optical, wettability, photocatalytic and morphological properties#288331
- Impact of Substrate Temperature on Sprayed Mo-doped ZnO Thin Films#442718
- Synthesis and Characterization of ZnO Nanorod Films on PET for Photocatalytic Disinfection of Water#1168283
- Control of NLO and photocatalysis properties based on the use of Sn-doped ZnO thin films for optoelectronics applications#354092
Record · ID 1100014
Retrieved via Conceptio: every document is proof-bundled with source, license, and retrieval metadata.
Retrieved via Conceptio: every document is proof-bundled with source, license, and retrieval metadata.
Bring this data into your agent: Connect via MCP or API · 20 free credits to start · no card required
Read the Docs → · View CLI source on GitHub · Conceptio Open Knowledge Archive
Read the Docs → · View CLI source on GitHub · Conceptio Open Knowledge Archive