Severe plastic deformation of an additively manufactured Ti–6%Al–4%V alloy: Effect of post-processing heat treatment and hot isostatic pressing on the behavior over a wide range of strain
A B S T R A C T Ti-6Al-4V (wt.%) alloy containing 0.14 wt.% trace Fe and 1 wt.% yttria-stabilized zirconia (YSZ) was manufactured by laser powder bed fusion. In addition to the as-built samples (AB), some samples received post-heat treatments, either by conventional heat treatment (HT) alone
Conceptio Open Archive
Analyze & explore related research in Conceptio
Connect this record directly into your research workflow or AI agent. Explore citations across open repositories, query full text, and export structured proof bundles.
This document is indexed with metadata only: full text is not available in the archive for this record. Open the official source ↗
Related documents
- Study the behaviour of Ti-Mo-xZr alloys during thermomechanical treatment.#14920
- Direct chill and electromagnetic casting of aluminium alloys: Thermomechanical effects and solidification aspects#445120
- Metal Segregation During the Solidification of Titanium-Aluminum Alloys for 3D Printing Applications#939003
- Influence of the Rapid Thermal Nitriding Process on the Properties of TiN Thin Films Obtained from TiO<sub>2</sub> Sol–Gel Layers#304534
- Development of a new high-strength diffusion-assisted healable Al-Mg-Zr alloy produced by powder bed fusion - laser beam/Metals#344551
Record · ID 1425818
Retrieved via Conceptio: every document is proof-bundled with source, license, and retrieval metadata.
Retrieved via Conceptio: every document is proof-bundled with source, license, and retrieval metadata.
Bring this data into your agent: Connect via MCP or API · 20 free credits to start · no card required
Read the Docs → · View CLI source on GitHub · Conceptio Open Knowledge Archive
Read the Docs → · View CLI source on GitHub · Conceptio Open Knowledge Archive