HAL (France)
open access
Cyclic behavior of a γ’ precipitation-hardened nickel-base superalloy: Fundamental strengthening mechanisms impacted by hydrogen
Conceptio Open Archive
Analyze & explore related research in Conceptio
Connect this record directly into your research workflow or AI agent. Explore citations across open repositories, query full text, and export structured proof bundles.
This document is indexed with metadata only: full text is not available in the archive for this record. Open the official source ↗
Related documents
- Mechanisms of Ordered Gamma Prime Precipitation in Nickel Base Superalloys#456420
- Mobility and trapping of hydrogen in high-strength steel#427234
- Green hydrogen support with overlapping climate policies#226538
- Study on the behavior of sustainable concrete using raw-crushed wind turbine blade and recycled concrete aggregate: optimization by response surface method#236899
- Carbon Dots for Corrosion Protection: A Systematic Review of Applications and Mechanisms.#140631
Record · ID 153877
Retrieved via Conceptio: every document is proof-bundled with source, license, and retrieval metadata.
Retrieved via Conceptio: every document is proof-bundled with source, license, and retrieval metadata.
Bring this data into your agent: Connect via MCP or API · 20 free credits to start · no card required
Read the Docs → · View CLI source on GitHub · Conceptio Open Knowledge Archive
Read the Docs → · View CLI source on GitHub · Conceptio Open Knowledge Archive