HAL (France)
open access
High‑throughput nanoindentation for the mechanical characterization of bearing steel subjected to fretting mechanisms
Conceptio Open Archive
Analyze & explore related research in Conceptio
Connect this record directly into your research workflow or AI agent. Explore citations across open repositories, query full text, and export structured proof bundles.
This document is indexed with metadata only: full text is not available in the archive for this record. Open the official source ↗
Related documents
- Rust-accelerated powder X-ray diffraction simulation for high-throughput and machine-learning-driven materials science.#433865
- Molecular Dynamics Simulation of the Grain Growth in Nano-Grained Metallic Polycrystals#69531
- Effects of interdot dipole coupling in mesoscopic epitaxial Fe(100) dot arrays#928996
- Engineered hierarchical 3D scaffold promotes bone regeneration through enhanced mechanotransduction.#360739
- State monitoring of rolling bearings in vibration-based anchor drilling rig based on machine learning model.#295287
Record · ID 202642
Retrieved via Conceptio: every document is proof-bundled with source, license, and retrieval metadata.
Retrieved via Conceptio: every document is proof-bundled with source, license, and retrieval metadata.
Bring this data into your agent: Connect via MCP or API · 20 free credits to start · no card required
Read the Docs → · View CLI source on GitHub · Conceptio Open Knowledge Archive
Read the Docs → · View CLI source on GitHub · Conceptio Open Knowledge Archive