Development of ferritic BCC-superalloys for high-temperature and nuclear applications

von Tiedemann, Sophia Olympia
UBIRA ETheses · Papers
Open Source ↗Direct PDF ↓
Advances in nuclear reactor technology, such as the ongoing development of nuclear fusion and generation-IV fission reactors, drive up operating temperatures (550°C to 1000°C) to increase thermodynamic efficiency, and require materials capable of withstanding highenergy neutron fluxes over prolonged
Conceptio Open Archive

Analyze & explore related research in Conceptio

Connect this record directly into your research workflow or AI agent. Explore citations across open repositories, query full text, and export structured proof bundles.

This document is indexed with metadata only: full text is not available in the archive for this record. Open the official source ↗

Related documents

Record · ID 824347
Retrieved via Conceptio: every document is proof-bundled with source, license, and retrieval metadata.
Bring this data into your agent: Connect via MCP or API · 20 free credits to start · no card required
Read the Docs → · View CLI source on GitHub · Conceptio Open Knowledge Archive